Feritna EE jezgra

Feritna EE jezgra

product-438-285

 

MODEL Bruto težina

Veličina (mm)

A

Bmin

C

D

E

F

EEL27

33

27.0±0.6

19.0 min

7.8±0.25

10.5±0.3

11.5±0.25

15.5±0.25

EE28

24

28.0±0.6

18.6

7.2±0.2

10.7±0.3

6.5±0.3

10.5±0.3

EE28.5

23

28.8±0.6

21.1

7.2±0.2

10.4±0.2

6.5±0.3

10.5±0.3

EE30/7

24

30.0±0.5

19.9±0.4

6.9±0.3

7.1±0.2

10.0±0.2

15.0±0.2

EE32/9.5

36

32.1±0.5

22.7

9.5±0.3

9.5±0.2

11.5±0.3

16.4±0.2

EE32/11

42

32.1±0.5

22.7

9.5±0.3

11.0±0.2

11.5±0.3

16.4±0.2

EE32.6/37/9.5

40

32.6±0.5

23.6

9.5±0.3

9.5±0.2

14.3±0.3

18.6±0.3

EE33A

42

34.0±0.5

24

9.6±0.3

12.7±0.3

9.8±0.3

14.1±0.3

EE35/18

45

35.0±0.6

24.6

10.0±0.3

10.0±0.3

12.5±0.3

17.5±0.3

EE35/28

33

34.2±0.6

24

9.5±0.3

10.0±0.3

9.2±0.3

13.7±0.3

EE42/15/21

93

42.1±0.9

29.5

12.0±0.3

15.0±0.3

15.2±0.4

21.1±0.3

EE42/20/21

121

42.1±0.9

29.5

12.0±0.3

19.7±0.4

15.2±0.4

21.1±0.3

EE42/15/50

108

42.1±0.9

29.5

12.0±0.3

15.0±0.3

19.0±0.4

25.0±0.3

EE50

120

50.0±0.7

34.2

14.6±0.4

14.6±0.4

13.1±0.3

21.5±0.3

EE55A

186

55.1±1.1

37.5

17.0±0.3

16.9±0.3

18.8±0.3

27.5±0.3

EE55B

230

55.1±1.1

37.5

17.0±0.3

20.7±0.3

18.8±0.3

27.5±0.3

EE55C

272

55.1±1.1

37.5

17.0±0.3

24.7±0.3

18.8±0.3

27.5±0.3

EE65A

304

65.2±1.3

44.2

19.6±0.3

19.6±0.3

22.5±0.3

32.5±0.3

EE65B

416

65.2±1.3

44.2

19.6±0.3

27.0±0.3

22.5±0.3

32.5±0.3

EE70A

412

70.5±1.5

48.0

16.7±0.5

24.5±0.6

24.6±0.6

35.5±0.5

EE70B

530

70.7±1.5

48.0

21.5±0.5

30.5±0.6

22.0±0.6

32.0±0.4

EE70/72

418

70.0±1.5

48.0

16.7±0.5

24.5±0.6

27.0±0.6

36.3±0.4

EE73/70

570

73.0±1.5

50.0

21.5±0.5

30.5±0.6

24.3±0.6

35.0±0.4

EE80/38/20

396

80.7±2.0

59.1

20.0±0.5

20.0±0.6

28.0±0.5

38.0±0.5

EE85A

726

85.0±3.0

55.0

27.0±0.4

26.5±0.5

29.0±0.5

44.0±1.0

EE85B

860

85.0±3.0

55.0

27.0±0.4

31.5±0.5

29.0±0.5

44.0±1.0

EE100

1173

100.0+3.0/-1.5

72.0min

28.0±0.5

28.0±0.5

46.0±0.5

60.0±0.5

EE110

1700

110.0±3.0

74.2

36.0±1.0

36.0±1.0

38.7±0.6

57.0±0.5

EE130

2410

130.0±3.0

89.0

40.0±2.0

40.0±1.0

43.0±0.8

63.0±1.0

EE160

3400

160.0±3.0

120.0

40.0±2.0

20.0±1.5

64.0±1.0

83.0±1.0

EE188

6880

185.0±3.5

128.0

55.5±2.5

55.0±2.0

49.0±1.5

79.0±1.5

EE193

6880

193.0±3.5

132.0

58.0±2.0

59.0±2.0

49.0±1.5

79.0±1.5

EE210

5620

210.0±3.5

149.0

58.0±2.0

40.0±1.0

65.0±1.5

95.0±1.5

EE240

7000

240.0±4.0

176.0

56.0±3.0

40.0±1.5

86.5±1.0

117.0±1.0

 

 

MODEL

Specifikacija

AL±25%(nH/N^2)

NETO TEŽINA (g)

C1mm-1

Lemm

Aemm2

Vemm3

ZP40

ZH5K

ZH7K

ZH10K

CEEL27

0.867

70.0

80.7

5650.0

2500

27.0

EE28

0.620

51.7

82.9

4290.0

3500

21.6

EE28.5

0.660

51.4

77.6

4000.0

3300

21.0

EE30

1.089

65.4

60.0

3920.0

1980

19.4

EE32/9.5

0.890

74.6

86.3

6440.0

2500

32.0

EE32/11

0.746

74.6

100.0

7450.0

2900

37.5

EE32.6/37/9.5

1.026

85.5

83.0

7150.0

2200

36.0

EE33A

0.589

67.4

114.0

7690.0

3700

39.0

EE35/18

0.810

80.7

100.0

8070.0

2700

41.0

EE35/28

0.753

67.7

89.9

6090.0

2900

30.0

EE42

0.534

97.0

182.0

17600.0

4700

86.0

EE42A

0.415

97.4

235.0

22900.0

6100

115.0

EE42/15/50

0.630

113.0

179.0

20227.0

3400

100.0

EE50

0.425

95.8

226.0

21600.0

6100

115.0

EE55A

0.432

123.0

285.0

35050.0

5000

168.0

EE55B

0.348

123.0

354.0

43700.0

6500

220.0

EE55C

0.292

123.0

422.0

52130.0

7200

260.0

EE65A

0.373

146.8

393.1

57728.4

5800

280.0

EE65B

0.274

147.0

535.0

78700.0

7800

380.0

EE70

0.344

159.0

409.0

73200.0

6500

380.0

EE70B

0.226

150.0

665.0

99800.0

9000

500.0

EE70/72

0.360

161.0

409.0

65800.0

10000

388.0

EE73/70

0.236

159.0

665.0

106000.0

9000

560.0

EE80/38/20

0.469

184.0

392.0

72300.0

6000

360.0

EE85A

0.264

188.0

714.0

134000.0

8300

660.0

EE85B

0.220

189.0

859.0

162000.0

10000

750.0

EE100

0.344

270.000

784.000

222656.0

7300

1060.0

EE110

0.191

244.0

1280.0

312000.0

11000

1520.0

EE130

0.352

284.0

1600.0

454000.0

12000

2190.0

EE160

0.498

398.0

1600.0

637000.0

9000

2500.0

EE188

0.100

370.0

2940.0

1087800.0

21000

5700.0

EE193

0.100

380.0

3580.0

1360400.0

21000

5800.0

EE210

0.183

440.0

2400.0

1128000.0

13500

5400.0

EE240

0.235

556.4

2359.0

1312421.0

12500

5900.0

Popularni tagovi: feritne ee jezgre, Kina feritne ee jezgre proizvođači, dobavljači, tvornica

Pošaljite upit

(0/10)

clearall