Generally speaking, the silicon steel sheet of the stator itself has an insulation coating. As long as it is not in a special environment, its interlayer is not easily corroded. However, on the stamping shear surface of the stator and rotor, due to the direct interaction between Fe and air, if rust prevention treatment is not carried out immediately after stamping, the iron core will generally rust to varying degrees within 1-2 weeks; But even if rust prevention treatment is used, if the working environment of the motor is too long or there is water mist, such as the motor of the plant protection machine, special rust prevention treatment needs to be carried out for the product; We also call it electrophoretic spraying;
Thickness: {{0}}.013-0.025mm, with a maximum thickness of 0.1mm
Rust prevention ability: can pass 24-hour salt spray test;